Can you weld cracked rims?
I guess its not a good idea but can it be done sorry for the short one not time!!!
|
5 Apr 2008
|
|
Registered Users
Veteran HUBBer
|
|
Join Date: Oct 2003
Location: Vancouver, BC, for now...
Posts: 792
|
|
Yes, if your a really good welder.
|
7 Apr 2008
|
|
Registered Users
Veteran HUBBer
|
|
Join Date: Oct 2003
Location: Vancouver, BC, for now...
Posts: 792
|
|
Nearly all rims are welded. They start as flat stock and are rolled, cut to size then welded together. If they are cast, you may run into some problems, depending on the quality of the material used. Take it in to a good welding shop and some welding and grinding should fix you up.
|
7 Apr 2008
|
|
Registered Users
Veteran HUBBer
|
|
Join Date: Oct 2003
Location: Vancouver, BC, for now...
Posts: 792
|
|
Reguarding the Dura-fix rod, i would not recomend it for a rim. It doesn't penetrate the base metal well enough to provide a good weld. It's more like glue, or brazing for aluminum if you will. TIG is the way to go for aluminum, but a spool gun (wire feed) will work fine also. BTW, what are you trying to weld?
|
8 Apr 2008
|
|
Large Golden Member
Veteran HUBBer
|
|
Join Date: Aug 2005
Location: BC, Canada
Posts: 1,085
|
|
Yes rims can be welded BUT whether or not they SHOULD be depends upon the type of damage sustained .
Assuming the rim is aluminum:
Mr Ron is correct ,AC Tig is the best way to go , Mig maybe would do the job but might not penetrate well enough ,it depends upon the skill of the welder .If the rim is thoroughly prepared and all oxidation removed ,preheated and restrained during welding then there should not be any problem .
Durafix would be a definate no no in my book .
__________________
Blessed are the cracked, for they let in the light. - Spike Milligan
"When you come to a fork in the road ,take it ! When you come to a spoon in the road ,take that also ."
|
8 Apr 2008
|
|
Gold Member
Veteran HUBBer
|
|
Join Date: Mar 2006
Posts: 211
|
|
Thanks for all your replys guys, this is why I love the hubb! Just heading in to Dae es Salam now to go find some TIG or MIG welding! Yer they are alloy rims off a TT600RE. two cracks about 6/7mm long on the edge of the rim. I know I a good enginer who hopefuly know a good welder!
Thanks again for all you help.
George
Trans-Africa 07/08.
|
9 Apr 2008
|
Registered Users
Veteran HUBBer
|
|
Join Date: Apr 2003
Location: Manchester UK
Posts: 235
|
|
Quote:
Originally Posted by Mr. Ron
Reguarding the Dura-fix rod, i would not recomend it for a rim. It doesn't penetrate the base metal well enough to provide a good weld. It's more like glue, or brazing for aluminum if you will. TIG is the way to go for aluminum, but a spool gun (wire feed) will work fine also. BTW, what are you trying to weld?
|
You are absolutely right, no argument there. I was refering to filling a crack as a temporary measure to prevent tube pinch etc. I tig weld aluminium on a hobbyist level, and I can assure you, I would not attempt to tig weld the rims in an emergency. For starters, you cannot be sure of what alloy is being used in the rim, and whether it is weldable or not. Secondly, what filler rod to use 5xxx or 4xxx. Thirdly the amperage to weld that thickness of aliminium would be at least in the 150 to 200 Amp mark for penetration. Ali melts at about 800 degree C, the ali oxide at 1300 degree C, dura weld at 380 degree C. Much more room for error. At those tig temps a buckle or deformatity is guarranteed unless the wheel is preheated in a oven and restrained. All in all, this is a specialist job. Not something done in an emergency as a quick fix, as it could very quickly become a quick bin job.
|
13 Apr 2008
|
|
Registered Users
Veteran HUBBer
|
|
Join Date: Sep 2006
Location: At the moment:Zanzibar
Posts: 116
|
|
how´s it going?
How´s it going with the rim repairs? I have a new 18" rim laying around for my Tenere that I haven´t had time to spoke yet. Im on Zanzibar, so if you are geting no where with your fix and need help send me a Pm.
Tom
__________________
Places to be and things to do, see you all out there!!
Cheers.
Tom.
|
Currently Active Users Viewing This Thread: 3 (0 Registered Users and/or Members and 3 guests)
|
|
Posting Rules
|
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts
HTML code is Off
|
|
|
|
Check the RAW segments; Grant, your HU host is on every month!
Episodes below to listen to while you, err, pretend to do something or other...
2020 Edition of Chris Scott's Adventure Motorcycling Handbook.
"Ultimate global guide for red-blooded bikers planning overseas exploration. Covers choice & preparation of best bike, shipping overseas, baggage design, riding techniques, travel health, visas, documentation, safety and useful addresses." Recommended. (Grant)
Ripcord Rescue Travel Insurance™ combines into a single integrated program the best evacuation and rescue with the premier travel insurance coverages designed for adventurers.
Led by special operations veterans, Stanford Medicine affiliated physicians, paramedics and other travel experts, Ripcord is perfect for adventure seekers, climbers, skiers, sports enthusiasts, hunters, international travelers, humanitarian efforts, expeditions and more.
Ripcord travel protection is now available for ALL nationalities, and travel is covered on motorcycles of all sizes!
What others say about HU...
"This site is the BIBLE for international bike travelers." Greg, Australia
"Thank you! The web site, The travels, The insight, The inspiration, Everything, just thanks." Colin, UK
"My friend and I are planning a trip from Singapore to England... We found (the HU) site invaluable as an aid to planning and have based a lot of our purchases (bikes, riding gear, etc.) on what we have learned from this site." Phil, Australia
"I for one always had an adventurous spirit, but you and Susan lit the fire for my trip and I'll be forever grateful for what you two do to inspire others to just do it." Brent, USA
"Your website is a mecca of valuable information and the (video) series is informative, entertaining, and inspiring!" Jennifer, Canada
"Your worldwide organisation and events are the Go To places to for all serious touring and aspiring touring bikers." Trevor, South Africa
"This is the answer to all my questions." Haydn, Australia
"Keep going the excellent work you are doing for Horizons Unlimited - I love it!" Thomas, Germany
Lots more comments here!
Diaries of a compulsive traveller
by Graham Field
Book, eBook, Audiobook
"A compelling, honest, inspiring and entertaining writing style with a built-in feel-good factor" Get them NOW from the authors' website and Amazon.com, Amazon.ca, Amazon.co.uk.
Back Road Map Books and Backroad GPS Maps for all of Canada - a must have!
New to Horizons Unlimited?
New to motorcycle travelling? New to the HU site? Confused? Too many options? It's really very simple - just 4 easy steps!
Horizons Unlimited was founded in 1997 by Grant and Susan Johnson following their journey around the world on a BMW R80G/S.
Read more about Grant & Susan's story
Membership - help keep us going!
Horizons Unlimited is not a big multi-national company, just two people who love motorcycle travel and have grown what started as a hobby in 1997 into a full time job (usually 8-10 hours per day and 7 days a week) and a labour of love. To keep it going and a roof over our heads, we run events all over the world with the help of volunteers; we sell inspirational and informative DVDs; we have a few selected advertisers; and we make a small amount from memberships.
You don't have to be a Member to come to an HU meeting, access the website, or ask questions on the HUBB. What you get for your membership contribution is our sincere gratitude, good karma and knowing that you're helping to keep the motorcycle travel dream alive. Contributing Members and Gold Members do get additional features on the HUBB. Here's a list of all the Member benefits on the HUBB.
|
|
|